Sammanfattning
Polyurethane (PU) adhesives were prepared with bio-polyols obtained via acid-catalyzed polyhydric alcohol liquefaction of wood sawdust and polymeric diphenylmethane diisocyanate (pMDI). Two polyols, i.e., crude and purified liquefied wood (CLW and PLW), were obtained from the liquefaction process with a high yield of 99.7%. PU adhesives, namely CLWPU and PLWPU, were then prepared by reaction of CLW or PLW with pMDI at various isocyanate to hydroxyl group (NCO:OH) molar ratios of 0.5:1, 1:1, 1.5:1, and 2:1. The chemical structure and thermal behavior of the bio-polyols and the cured PU adhesives were analyzed by Fourier transform infrared spectroscopy (FTIR) and thermogravimetric analysis (TGA). Performance of the adhesives was evaluated by single-lap joint shear tests according to EN 302-1:2003, and by adhesive penetration. The highest shear strength was found at the NCO:OH molar ratio of 1.5:1 as 4.82 & PLUSMN; 1.01 N/mm(2) and 4.80 & PLUSMN; 0.49 N/mm(2) for CLWPU and PLWPU, respectively. The chemical structure and thermal properties of the cured CLWPU and PLWPU adhesives were considerably influenced by the NCO:OH molar ratio.
| Originalspråk | Engelska |
|---|---|
| Artikelnummer | 3267 |
| Antal sidor | 18 |
| Tidskrift | Polymers |
| Volym | 13 |
| Nummer | 19 |
| DOI | |
| Status | Publicerad - 2021 |
FN:s SDG:er
Detta resultat bidrar till följande hållbara utvecklingsmål:
-
SDG 12 – Hållbar konsumtion och produktion
Nyckelord
- adhesive penetration
- bio-polyol
- bond strength
- ethylene glycol
- FTIR
- liquefaction
- pMDI
- TGA